WebJan 8, 2012 · Chitin is the second most abundant semicrystalline polysaccharide Like cellulose, the amorphous domains of chitin can also be removed under certain … WebNov 1, 2014 · Chitin microfibrils or whiskers with high surface areas and stiffness can be developed as tissue engineering scaffolds, wound dressing, metal ion adsorbent, packaging or edible film, separation membrane, sensor as well as biocomposites with high mechanical properties (Jayakumar et al. 2010; Ifuku and Saimoto 2012; Jin et al. 2013; Ifuku et al. …
Fabrication of α-chitin whisker-reinforced poly(vinyl alcohol ...
WebAug 21, 2006 · The α-chitin whiskers were prepared from α-chitin flakes from shrimp shells by acid hydrolysis. The as-prepared chitin whiskers exhibited lengths in the range 231–969 nm and widths in the range 12–65 nm, with the average length and width being about 549 and 31 nm, respectively. WebAug 15, 2024 · The liquid crystalline and rheological properties of chitin whiskers (CHWs) are significant for their application in fabrication of highly ordered composite materials and optical components. The aim of this work was to elucidate the influence of chemical structure and chargeability (zeta potential, electropositivity, electronegativity or ... imperial facility rates
Liquid crystalline and rheological properties of chitin …
WebJan 22, 2015 · Chitin whiskers are rod-like short fibers that have a high aspect ratio and possess a high degree of crystallinity, as can be seen from XRD pattern. This acts as contribution factor that increases the mechanical properties. According to past research (Ma et al., 2014) hydrogen bonding causes the composite film to exhibit higher modulus and ... WebThe α-chitin whiskers were prepared by acid hydrolysis of α-chitin from shrimp shells. The as-prepared whiskers exhibited the length in the range of 150–800 nm and the width in the range of 5–70 nm, with the average length and width … WebNov 1, 2015 · nanofibre film. Chitin whiskers suspension and 1 wt % PAA solution were gently mixed in beaker and magnetically stirred at room temperature for about 3-5 min maintaining the pH at 2. The solution... litcharts tuesdays with morrie